EVA film-EVA Film (High-End) Available products Production process (for reference only) To ensure product quality, the molding process is best carried out in two steps: The first step: Set the temperature at 60-65 degrees, and then keep it for 20-30 minutes after reaching this temperature. The purpose is to achieve the effects of "exhaust" and "dehumidification" while softening the film; Step 2: Set the temperature between 90 degrees and 95 degrees (depending on the specific situation), and then keep the temperature for 30-40 minutes, then let it continue to maintain vacuum in the furnace and naturally cool to about 60 degrees. And then the finished glass can be taken out. Special Note This reference process is based on a single-layer molding machine, and produces a 5 mm double-clip color transparent film glass as a production factor. The temperatureset is the surface temperature of the glass in the molding machine. Different m…