www.joyetv.com

MOR 2WSS Metal oxide film resistor

129

MOR 2WSS Metal oxide film resistor

Metal Oxide Film Resistor YZPST-MOR-2WSS-3K3-J The resistors arrayed are placed into a constant temp. humidity oven at the temp. of 40 ±2°c  and the humidity of 90~95%, then rated power is applied for 1.5 hours and cut off  for 0.5 hour. The similar cycle will be repeated for 500+24 -0 hours in total (including cut-off time). Then remove the voltage, taking the resistors out of the oven and leaving them at room temp. for one hour. The resistance value change rate between pre-and- post test shall be within ±5%. There also shall be no evidence of remarkable change on appearance, and the marking shall not be illegible.   TYPE   L    4   D t   H:t:3…